logo
Home Blog

How to Weld Dam Liners

Certification
China Hebei Boda Plastic Technology Co., Ltd. certification
China Hebei Boda Plastic Technology Co., Ltd. certification
Customer Reviews
Thank you very much. I hope we will make more Hydraulic Butt Fusion Machine Welding business in the future.

—— Mr Rusi

Thanks friend. It is a pleasure to deal with you.

—— Mr Walter

Thanks for the references, I see that you are a serious and reputable company.

—— Mr Dantas

I'm Online Chat Now
Company Blog
How to Weld Dam Liners
Latest company news about How to Weld Dam Liners

Welding is needed whenever a liner has to cover a water pan wider than the roll width: one roll covers a strip, and the strips have to be joined into a single sheet before the pan holds water. The method does not change with thickness or material; only the parameters do, which is why a dam liner welding machine is specified against the project, not against the roll.

A liner is welded either before installation, at the factory, or during installation, on site. Welding melts the liner at the joint, lays the two layers one over the other, and lets them harden into one unit. On HDPE the seam is fused at 0.5 to 4.0 mm; on PVC the same method runs at a lower temperature. Both materials in this guide carry UV stabilisation for intense tropical sunlight.

A geomembrane welder holds temperature, speed and pressure constant along the seam, which is what separates a factory weld from a field repair. The steps below follow the installation sequence, then the welding sequence.

Steps to Weld Dam Liners

1. Water Pan Excavation

Excavation comes first and usually takes the longest. It is done by hand with hand tools or by machine; the common machines are backhoe loaders, excavators and rollers. The side walls are cut at an incline so they do not collapse, and the floor is shaped to the pan profile the liner has to follow.

2. Smoothening the Water Pan

Smoothening removes anything sharp that would puncture the liner: tree stumps, stones, rocks and sharp sticks. Water the floor and the sides to soften the ground, then run a roller over it to compact the surface while smoothing it. A liner laid on a rough bed fails at the point of the stone, not at the seam.

3. Trench Making

Trenches are dug around the reservoir, and the liner is tucked into them so the edge cannot pull out. The size depends on the dam and on liner thickness; the common sizes are 30 cm by 30 cm and 45 cm by 45 cm. Sand bags along the top edge are the alternative where a trench is impractical.

Welding shapes the pond liner welding machine work to the geometry of the pan. The welded joints have to be leak-free for the liner to hold water at all, and lined pans are the storage unit for irrigation in a climate with one or two rainy seasons.

How to Weld Dam Liners: Factory and Field

1. Factory Welding

Depending on the size of the liner, it is welded whole or partially at the factory. The weight and volume of the welded piece have to stay portable on site, and that limit decides how much of the liner is joined before it ships. A hot wedge welder in the CX600 class runs a 1 mm sheet at 0 to 9 m/min, so a full roll is joined in a single pass rather than in sections.

2. Site or Field Welding

Field welding happens at the point of installation, joining the factory panels into the finished liner. It is needed when the whole liner cannot be assembled at the factory because of weight or bulk, which is the usual case on a large pan. The thicker the liner, the smaller the panel that stays portable, and the more of the work moves to site.

3. Equipment: Wedge Welder or Hot Air Welder

Two machines do the work. A wedge welder takes the factory seams and the long straight runs; a hot air welder is the portable unit for field joins, corners and repairs. In the CX range the factory machine is the CX600 at 2100 W for 0.8 to 4.0 mm, or the CX700 at 2400 W when the liner runs to 3 mm and the seams are long; the field machine is the CX1600S at 1600 W, 20 to 620 °C and 160 L/min, with slot, tubular and angle nozzles for laps, pipe work and corners.

The two machines leave different seams. A hot wedge welder lays two parallel tracks with an enclosed air channel between them, and that channel is a test port: pressure it, watch the gauge, and an unbroken seam proves itself over its full length. A hot air weld is a single bead, checked by vacuum box or by pulling a coupon. Where the specification calls for a pressure-tested seam, the wedge is the method; where the work is thin film, PVC or a corner a wedge cannot reach, the hot air plastic welder is the method.

Both run on electric power. An off-grid site needs a generator sized to the machine: 1400 to 2400 W for a dam liner welding machine in the CX600 or CX700 class, 1600 W for the CX1600S. Undersizing the generator shows up as a seam that stalls halfway, not as a machine that refuses to start.

4. Seam Testing and Repair

A finished liner is proved, not assumed. The air channel is pressured with the CX-002 tester and read against the holding period; a vacuum hood covers the bead where there is no channel; a pulse-voltage detector scans the floor of the pan for pinholes. Where a seam fails, a hand extruder rebuilds the joint: the CX800A runs an 800 W auger at 2 to 2.5 kg/h on 3 to 5 mm rod, the CX800B a 1300 W auger at 2 to 3 kg/h, and both cover 1 to 20 mm material, which takes in pipe boots, patches and field damage.

An hdpe liner welding machine working at 1.5 mm leaves a seam at 85 per cent of base material or better. That figure, not the machine price, is what the client is buying.

Pub Time : 2026-11-27 15:36:24 >> Blog list